The Recall Desk

Hazard

Weld Crack recalls

16 recalls in our database tag this hazard, drawn from FDA, USDA FSIS, CPSC, and NHTSA source notices.

What the numbers show

Total
16
Critical
0
Severe
0
Most recent
2024-07-03

Of the 16 weld crack recalls we have scored against our rubric, 0 (0%) are Critical — deaths or serious injuries reported, or the agency’s own highest classification — and 0 (0%) are Severe.

About this hazard tag

Hazard tags are short, machine-readable labels we attach to every recall to make cross-cutting queries possible — “all weld crack recalls regardless of agency”, “all listeria recalls in California”, “all airbag recalls in 2025”. The tags are extracted from each recall’s source text during the LLM rewrite step and validated against a fixed schema.

A recall can carry multiple tags — a Listeria recall might also be tagged ready-to-eat and undeclared-allergen. Use the full-text search if you want to combine hazard tags with brand or category filters.

1–16 of 16

  • HighFDA (Devices)·Z-2191-2024·2024-07-03

    Medtronic COBALT XT HF CRT-D implantable defibrillator recalled for manufacturing defects

    Medtronic is recalling 8 units of the COBALT XT HF CRT-D MRI SureScan implantable cardioverter defibrillator due to manufacturing defects identified during quality control testing.

    Product
    COBALT XT HF CRT-D MRI SureScan, Model Number: DTPA2D1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2193-2024·2024-07-03

    Implantable Defibrillator Recalled for Manufacturing Weld Crack Defect

    Medtronic is recalling 11 units of the COBALT XT HF QUAD CRT-D MRI SureScan implantable cardioverter defibrillator due to a manufacturing defect involving weld cracks that failed quality control testing.

    Product
    COBALT XT HF QUAD CRT-D MRI SureScan, Model Number DTPA2Q1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2207-2024·2024-07-03

    Medtronic COBALT DR MRI SureScan ICD Recalled Due to Manufacturing Weld Crack

    Medtronic is recalling 36 COBALT DR MRI SureScan implantable cardioverter defibrillators due to a weld crack manufacturing defect. The defect was identified during manufacturing quality checks.

    Product
    COBALT DR MRI SureScan, Model Number DDPB3D4, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2209-2024·2024-07-03

    Implantable defibrillator recalled for manufacturing defect causing device failure risk

    Medtronic is recalling five implantable defibrillators due to a manufacturing defect where weld cracks caused devices to fail quality testing. The defective devices were identified during manufacturing and did not reach patients.

    Product
    Cobalt XT DR MRI SureScan, Model Number DDPA2D1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2206-2024·2024-07-03

    Medtronic COBALT DR MRI ICD Recalled for Manufacturing Defect

    Nine Medtronic COBALT DR MRI implantable cardioverter defibrillators are recalled due to a weld crack that caused devices to fail manufacturing quality checks.

    Product
    COBALT DR MRI SureScan, Model Number DDPB3D1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2212-2024·2024-07-03

    Medtronic Implantable Defibrillators Recalled for Manufacturing Weld Defect

    Medtronic is recalling 82 implantable cardioverter defibrillators due to a manufacturing defect involving weld cracks discovered during quality control testing before distribution to patients.

    Product
    Product not distributed in the US. Implantable Cardioverter Defibrillators: a. VIVA QUAD XT CRT-D, Model Number DTBA2QQ. b. CLARIA MRI CRT-D SureScan, Model Number DTMA2D1. c. CLARIA MRI QUAD CRT-D SureScan, Model Number DTMA2QQ. d. AMPLIA MRI CRT-D SureScan…
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2204-2024·2024-07-03

    Medtronic Implantable Cardioverter Defibrillator Recalled Due to Weld Crack Defect

    Medtronic is recalling 6 units of the MIRRO MRI VR SureScan implantable cardioverter defibrillator due to a potential manufacturing defect. The devices failed manufacturing quality checks because of a weld crack.

    Product
    MIRRO MRI VR SureScan, Model Number DVME3D1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2200-2024·2024-07-03

    Medtronic PRIMO MRI DR SureScan Cardioverter Defibrillators Recalled for Manufacturing Defect

    Medtronic is recalling two PRIMO MRI DR SureScan implantable cardioverter defibrillators due to a potential manufacturing defect involving weld cracks detected during manufacturing quality testing.

    Product
    PRIMO MRI DR SureScan, Model Number DDMD3D1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2199-2024·2024-07-03

    Implantable Cardioverter Defibrillator with Weld Crack Defect Recalled

    Medtronic is recalling 40 EVERA MRI S DR SureScan ICDs (Model DDMC3D4) due to manufacturing weld cracks that caused devices to fail leak tests. The defect was identified during manufacturing; no patient harm has been reported.

    Product
    EVERA MRI S DR SureScan, Model Number DDMC3D4, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2192-2024·2024-07-03

    Medtronic Implantable Defibrillator Recalled Due to Manufacturing Weld Crack

    Medtronic is recalling 14 Cobalt XT HF CDT-D MRI SureScan implantable defibrillators due to a manufacturing weld defect that could cause device failure.

    Product
    Cobalt XT HF CDT-D MRI SureScan, Model Number: DTPA2D4, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2205-2024·2024-07-03

    Medtronic MIRRO MRI ICD devices recalled for manufacturing weld crack defect

    Medtronic recalls 13 MIRRO MRI VR SureScan implantable cardioverter defibrillators (ICDs) due to a manufacturing weld crack. The defect was identified and caused device failure during the manufacturing leak check quality control test.

    Product
    MIRRO MRI VR SureScan, Model Number DVME3D4, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2203-2024·2024-07-03

    Implantable Cardioverter Defibrillator Recalled for Manufacturing Weld Defect

    Medtronic recalls 46 PRIMO MRI VR SureScan implantable cardioverter defibrillators due to a manufacturing defect. Weld cracks identified during manufacturing quality checks could cause device failure.

    Product
    PRIMO MRI VR SureScan, Model Number DVMD3D4, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2201-2024·2024-07-03

    Medtronic MIRRO MRI implantable defibrillator recalled for weld defect

    Medtronic is recalling 3 MIRRO MRI DR SureScan implantable cardioverter defibrillators due to a manufacturing weld crack that caused devices to fail quality checks. The defect was detected during manufacturing before devices reached patients.

    Product
    MIRRO MRI DR SureScan, Model Number DDME3D1, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2190-2024·2024-07-03

    Medtronic Implantable Cardioverter Defibrillator Recalled for Manufacturing Weld Defect

    Medtronic recalled 14 COBALT HF QUAD CRT-D MRI SureScan implantable defibrillators due to a weld crack manufacturing defect detected during quality control testing.

    Product
    COBALT HF QUAD CRT-D MRI SureScan, Model Number DTPB2QQ, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2208-2024·2024-07-03

    Medtronic COBALT VR MRI SureScan implantable defibrillators recalled for manufacturing defect

    Medtronic is recalling 4 COBALT VR MRI SureScan implantable cardioverter defibrillators due to a manufacturing defect involving a weld crack identified during quality control testing.

    Product
    COBALT VR MRI SureScan, Model Number DVPB3D4, Implantable Cardioverter Defibrillator
    Category
    Medical Device
    Distribution
    Distributed nationwide
  • HighFDA (Devices)·Z-2481-2023·2023-09-06

    Surgical Rasp Handle May Fracture Due to Weld Crack

    The Link OptiStem Rasp Handle used in knee replacement surgery may develop a crack in the weld that causes the handle to fracture. If this occurs, surgical removal of the rasp must be modified, potentially prolonging the procedure.

    Product
    Link OptiStem Rasp Handle-Used with the OptiStem Rasp to prepare the femoral medullary canal for a knee prosthesis implant during a total knee arthroplasty surgical procedure Item Number: 17-5220/01
    Category
    Medical Device
    Distribution
    3 states